On the plant drawing, the coal route is one line from unloading to bunker. At the transfer house it is anything but one duty. A rock in wet run-of-mine coal hits the receiving belt. Farther on, screened coal leaves a dusty stripe on a fast return. A biomass feeder brings its own fines and awkward pieces of wood. A hot ash conveyor belongs on a different page again.
Before asking a supplier for a single replacement specification, mark the failed belt's position on that drawing. Put the material state beside it. The same tonnes per hour can hide very different problems at the skirt, cleaner and tail pulley. SINOCONVE manufactures the belts and supplies the surrounding components through qualified partners. For a useful enquiry we need the line condition, not only its annual tonnage.
Send the route sketch and the failed-belt photographs
The first receiving belt gets whatever came through the unloading hopper. Rain may have left one load soft and muddy. A hard piece in the next load might strike the belt at the same hopper lip. Go there with the removed belt section. Is the first cut directly below that lip, or farther along under the skirt? Measure the gap between support rolls at the mark; the boiler rating is no help with that measurement.
Take a photograph with the hopper lip and support station in frame. Measure the lump size actually found there and the loaded belt sag. Do not copy a maximum lump size from an old project sheet without checking the current screening arrangement. The impact and cut resistant belt is one construction to compare after the landing is understood; a thicker cover cannot prevent a sharp object from lodging under a tight skirt.
Farther down the route, screened coal may leave dust on the head pulley with hardly a dent in the cover. The reclaim scraper, meanwhile, may be dragging a sticky layer left by the last rain. Put the head pulley and scraper photos beside the hopper photo. Now the three marks can be tied to three conveyor IDs on the drawing.
| Position | What arrives on the belt | First place to inspect |
|---|---|---|
| Unloading hopper | Mixed lumps and fines, variable water | Chute exit, skirt and support |
| Stockpile reclaim | Wet fines and occasional compacted material | Cleaner, return rollers and tail |
| Screened bunker feed | Smaller coal and airborne dust | Seals, scraper strip and tracking |
| Biomass addition | Pellets, chips or fibrous pieces | Feed control and skirt pockets |
| Ash removal | Temperature and particle form vary by system | Separate process and belt review |
The last row is deliberately separate. A boiler ash stream may be wet, cooled or still hot depending on the plant and the handling system. It cannot be assigned the coal belt grade from a material name alone.
At the isolated reclaim head, take a little residue from the belt beyond the discharge. Crush a pinch against a white card. A gritty stain after rain is different from yesterday's loose granules. Write “reclaim head, wet shift” on the card and photograph the cleaner setting beside it. The blade may be in exactly the same position it held during dry weather.
Watch the return rollers during a guarded run. A sleeve of packed material on one shell changes the effective diameter beneath the belt. The belt may then wander into a bracket. The complaint may be an edge worn bright on one side, although the first oddity is the wet roller several stations earlier. Tag that station and collect the crust at the next isolated stop.
Before writing “poor cover” on the failure report, trace the water. Was the suppression spray changed? Is one drain now running into the transfer? Ask the fitter to show the cleaner's discharge tray. If wet fines are falling onto the tail run, an adjusted blade has moved the mess without removing it. The return idler range helps identify replacement hardware; specify the seal and carryback route too.
Dust tells a different story. A dry screened line can coat seal gaps without leaving much visible paste on the belt. If one idler is hard to turn after isolation, locate the dust leak upstream before replacing a row of otherwise sound rollers. Coal and biomass dust also require the plant's fire and housekeeping controls. A belt marked “fire resistant” is not a substitute for the site risk assessment; request the exact test standard and evidence required for that installation.
Stand where the primary blade meets the head pulley, behind guarding. Does one end skip the belt? Does the splice knock the blade once per lap? At the stop, put a chalk mark at each blade end and trace the corresponding lines on the cover. That tells the fitter whether the dark patch comes from a missed edge or from material arriving after the blade. If a shiny groove matches the blade exactly, check its force.
There may be only a narrow space between the head drum and first return idler. Put the proposed secondary blade on a scale sketch of that space. Will the belt be supported across its full width at the contact point? Can a worker reach the tensioner without leaning over the discharge? Where does the removed coal fall? Martin Engineering's coal plant example uses two cleaners, but it is the installed geometry that decides whether that arrangement fits here.
The skirt deserves the same attention. A piece held between skirt rubber and the moving cover can draw a long cut, starting exactly at the loading zone. At the next planned stop, lift the skirt and check for a trapped lump and a continuous wear line. Make the skirt gap and chute loading central to the repair note. Simply tightening the skirt after finding spillage may press the offending piece harder against the belt.
A sister cement plant may have a belt of the right width and strength on paper. It is still a poor shortcut. Clinker can arrive much hotter at its belt. The coal receiving point may instead have large lumps, rain-soaked fines and a dust-control enclosure. Compare what actually lands on each belt and the temperature there. “Both run 800 tonnes per hour” tells us nothing about those differences.
Keep the useful parts of the old drawing: centre distance, pulley sizes and take-up travel. Recheck cover compound, carcass flexibility, loading support, cleaner and fire-safety requirement against this coal route. A high heat grade chosen for clinker should not be assumed necessary for ambient coal. Conversely, the coal line's dust and ignition controls must not be dropped because the copied sheet says only “general purpose.”
On a mixed-fuel plant, do the same exercise for biomass. Pellets tend to roll differently from lumpy coal. Chips can bridge at a chute and leave a fibrous pocket at the skirt. Their bulk density, size distribution and actual feed rate belong in the capacity calculation. If the line alternates between coal and biomass, test the worst loading and transfer condition for each, including startup and low-flow periods.
The cement plant overview and port handling overview describe adjacent systems. They are useful references for equipment layout; the belt order still needs its own material duty sheet.
The request from operations says “another 200 tonnes per hour.” The first response may be a drive-speed change. Go to the loaded transfer first. Film the discharge at normal feed and at the present peak; put a ruler beside the skirt during an isolated check. Light pellets may scatter farther with speed, and a full chute may back up even while the belt still has room. A proposed width change also needs a drawing of the existing frames and pulley faces.
Put the coal and biomass densities in different boxes on the calculation sheet. Draw the pile as it lies on this trough, leaving the actual edge clearance. Use that loaded area with speed and bulk density for a capacity check. CEMA's belt-book pages explain the cross-section used. Now go back to the chute: if feed lands on the left shoulder, the neat central pile in the calculation never existed.
The incline's take-up is nearly out of travel? Put a photograph of its indicator on the sketch. The yard transfer may have the same throughput but far less lift. Have the drive engineer calculate the working tension for each, and write the smallest pulley diameter beside it. Only then compare fabric and steel cord, including the proposed splice. At the loading point, fix a sagging span with support rather than extra plies.
| RFQ input | Where to get it | Why it matters |
|---|---|---|
| Peak and normal feed | Operating records, not nameplate alone | Capacity margin and cleaner loading |
| Material density and size | Current coal and biomass samples | Loaded cross-section and chute behavior |
| Moisture and temperature | At the actual loading point | Cover, cleaning and fire review |
| Pulley and take-up | Photograph the size plate and indicator | Check bend and available travel |
The drive slips after a storm, yet it ran normally during a dry trial. Start with the take-up indicator and the drum face. Has lagging worn smooth? Is coal paste caught in its grooves? Write down whether the slip comes on startup, at full load or on an empty belt. Then have the drive design checked for wrap, tension and pulley diameter. Changing lagging material without that check may trade one problem for another at the cover.
At the receiving station, look for the support directly beneath the chute. During the isolated survey, place a straightedge along the expected belt path. Is there an unsupported span at the impact point? Record its length and the drop above it. An impact idler or a bed can then be compared against the space the frame actually offers. Width alone does not close the skirt gap.
On the return, a tracking device may guide the belt back toward centre. It will not remove a sleeve of wet coal on the preceding roller or repair a bent frame. Trace the first point of sideways movement, then decide whether an aligning idler is useful there. Rollers, pulleys and brackets are supplied as components through qualified partners; the belt construction is manufactured by SINOCONVE. The components range helps identify what needs a separate maker and model on the order.
Lay the removed belt beside the route sketch. Chalk “carry” and “return” on its two faces before rolling it away. One wide photograph should show the damaged length beside the frame; place the ruler by the cut for a second shot. Does the nick appear once each time the chalked splice comes round? Or does the belt receive a fresh mark at one fixed station? Those observations narrow the search.
| Mark on the belt | First check | What to change if confirmed |
|---|---|---|
| Cut begins under receiving skirt | Trapped lump and skirt pressure | Remove trapping point and repair skirt setup |
| Narrow polished track on underside | Stopped roller or fixed bracket | Replace damaged hardware and assess cover |
| Edge polished on one side | First wandering station, buildup and frame | Clear cause before adding tracking force |
| Groove follows scraper position | Blade alignment, pressure and support | Reset cleaner and inspect cover loss |
| Cracks near a pulley or splice | Bend diameter, joint condition and tension | Review construction and joining procedure |
The table gives the fitter a place to start, not a verdict. The same narrow stripe can be made by a blade or a locked roller, depending on which face is marked. Have the splice technician open a suspect joint. Put the rejected section in the maintenance store with its job number. A note saying “belt failed” will be useless at the next tender.
For a rubber belt enquiry, start with a copy of the route sketch. Circle the wet reclaim section and the biomass feed, then write the conveyor IDs beside them. The plant's required fire test goes on the order by its full standard number. Ash gets a separate sheet with a loading-point temperature and a note on the wet or dry process. Send SINOCONVE the sketch and failed-belt photographs.
No. Compare the receiving point with the screened bunker feed: lump impact, water and dust differ. The long incline also has a different tension calculation from a short transfer. Group belts only after the duty sheets agree.
Rain changes what the cleaner has to remove. During the next wet reclaim, collect a pinch from the return roller sleeve. Does the used cover beneath it look swollen, or merely coated? Have a rejected piece examined for compound condition and ply adhesion if swelling is suspected.
Sometimes. Test its actual feed and transfer first. Light pellets may roll or scatter where coal stays put; chips can bridge at a chute. Check density, size, fire controls and the belt's loaded shape before sharing a spare.
Stand behind the head guard and follow the falling coal. Some may land in the tray; some may miss and hit the return. Walk on to the skirt beyond the cleaner. If fresh coal appears there, the blade was not the last source of the dirt.
The calculation may allow it. Watch the loaded edge and discharge at the proposed speed, particularly with the lightest fuel. Check chute capacity, dust control, drive and cleaner rating. Width changes require a structure review too.
No single coal belt grade covers every ash system. Take the temperature where ash lands on the belt; the cooler outlet figure may be different. Tell the supplier whether this is a dry or wet ash route and send its own drawing.
Related Articles:
PRODUCTS

We are focusing on material handling, power transmission and industry application.